Welcome to Hengshui Jianfeng Engineering Rubber co., LTD.,

Bridge expansion joint construction and method

author: Jianfeng Engineering from: ԭ date: 2017/9/2 18:00:00 hit: 7665
Tips: The construction technology and methods are as follows:marking, cutting, marking, deck and asphalt c...

The construction technology and methods are as follows:

marking, cutting, marking, deck and asphalt concrete paving is completed, about cutting machine cutting. The asphalt concrete paving is completed, according to the reserved slot width or notch wide on each side about 5cm for cutting machine cutting.

on the basis of the actual bridge abutment (pier) at the center of the expansion joint line, then anti size to both sides according to the design requirements, from the joint center according to the actual abutment joints (the center line, and then back to the size of both sides according to the design requirements of line to the desired width on both sides of the pop-up construction, should pay attention to changes in line width abutment to both sides the pop-up construction required width (uniform design 60cm), we should pay attention to changes of abutment width; the line should be straight, to pay attention to changes of abutment width; the line should be straight, uniform width. Then use concrete cutting machine by drawing a line on the asphalt pavement joint cutting to ensure cutting; seam position, widthThe degree of consistency. Then use the concrete cutting machine by drawing a line on the asphalt pavement joint cutting; to ensure the cutting position, the painting line on Asphalt Pavement of the slit size accurate, vertical, straight, no defect. Accurate size, vertical, straight, no defect. The step of construction use "the two cut construction method at the cutting edge, the step of construction using the two slit method construction. The first time slot according to the construction requirements of variable line anti 5cm inward edge, the slit extends two times. The construction method of shrinkage after installation for detecting flatness, two slit to the requirement of crack width, to ensure the cutting edge of the order.After the device is installed, it is based on the detection of flatness, and then the two cut to the required seam width, so as to ensure the cutting edge of the cutting edge.

filler joint

  

contact us

TEL: +8613132415777
FAX: 86-318-8538660
Email: eric@prolianz.com
sales@prolianz.com
URL: http://www.prolianz.com
ADD: Hengshui City, Hebei Province, China

Copyright © 2016 Hengshui Jianfeng Engineering Rubber co., LTD., All Rights Reserved.
SITEMAP | XML | RSS